Researchers creating a safer, cleaner way to recover rare-earth metals from old phones and laptops

The date of: 2021-04-19
viewed: 27

source:Tech Xplore

Rare-earth metals are critical to the high-tech society we live in as an essential component of mobile phones, computers and many other everyday devices. But increasing demand and limited global supply means we must urgently find a way to recover these metals efficiently from discarded products.

Rare-earth metals are currently mined or recovered via traditional e-waste recycling. But there are drawbacks, including high cost, environmental damage, pollution and risks to human safety. This is where our ongoing research comes in.

Our team in collaboration with the research center Tecnalia in Spain has developed a way to use environmentally friendly chemicals to recover rare-earth metals. It involves a process called 'electrodeposition,' in which a low electric current causes the metals to deposit on a desired surface.

This is important because if we roll out our process to scale, we can alleviate the pressure on global supply, and reduce our reliance on mining.

The increasing demand for rare-earth metals

Rare-earth metals is the collective name for a group of 17 elements: 15 from the 'lanthanides series' in the periodic table, along with the elements scandium and yttrium. These elements have unique catalytic, metallurgical, nuclear, electrical, magnetic and luminescent properties.

The term 'rare' refers to their even, but scarce, distribution around the world, noted after they were first discovered in the late 18th century.

These minerals are critical components of electronic devices, and vital for many green technologies; they're in magnets for wind power turbines and in batteries for hybrid-electric vehicles. In fact, up to 600 kilograms of rare-earth metals are required to operate just one wind turbine.

The annual demand for rare-earth metals doubled to 125,000 tons in 15 years, and the demand is projected to reach 315,000 tons in 2030, driven by increasing uptake in green technologies and advancing electronics. This is creating enormous pressure on global production.

For example, recovering them from electric vehicle batteries involves traditional hydrometallurgical (corrosive media treatment) and pyrometallurgical (heat treatment) processes. But these have several drawbacks.

Pyrometallurgy is energy-intensive, involving multiple stages that require high working temperatures, around 1,000℃. It also emits pollutants such as carbon dioxide, dioxins and furans into the atmosphere.

Meanwhile, hydrometallurgy generates large volumes of corrosive waste, such as highly alkaline or acidic substances like sodium hydroxide or sulfuric acid.

Similar recovery processes are also applied to other energy storage technologies, such as lithium ion batteries.

Why our research is different

Given these challenges, we set out to find a sustainable method to recover rare-earth metals, using electrodeposition.

Electrodeposition is already used to recover other metals. In our case, we have designed an environmentally friendly composition based on ionic liquid (salt-based) systems.

We focused on recovering neodymium, an important rare-earth metal due to its outstanding magnetic properties, and in extremely high demand compared to other rare-earth metals. It's used in electric motors in cars, mobile phones, wind turbines, hard disk drives and audio devices.

Ionic liquids are highly stable, which means it's possible to recover neodymium without generating side products, which can affect the neodymium purity.

The novelty of our research using ionic liquids for electrodeposition is the presence of water in the mix, which improves the quantity of the final recovered neodymium metal.

Unlike previously reported methods, we can recover neodymium metal without using controlled atmosphere, and at working temperature lower than 100℃. These are key considerations to industrializing such a technology.

At this stage we have proof of concept at lab scale using a solution of ionic liquid with water, recovering neodymium in its most expensive metallic form in a few hours. We are currently looking at scaling up the process.

An important early step

In time, our method could avoid the need to mine for rare earth metals and minimizes the generation of toxic and harmful waste. It also promises to help increase economic returns from e-waste.

Importantly, this method could be adapted to recover metals in other end-of-life applications, such as lithium ion batteries, as a 2019 report projected an 11% growth per annum in production in Europe.

Our research is an important early step towards establishing a clean and sustainable processing route for rare-earth metals, and alleviating the pressures on these critical elements.



Hot News / Related to recommend
  • 2026 - 09 - 03
    Click on the number of times: 2
    The Synergistic Impact of Lanthanide-Doped Nickel Iron Sulphides (NiFeSs) Synthesized by a Hydrothermal Method for Effective Water and Urea Electrolysis in Anion Exchange Membranes来源:ACS PublicationsO...
  • 2026 - 09 - 03
    Click on the number of times: 2
    来源:ACS PublicationsMixed valency in compounds containing rare-earth elements can lead to intriguing properties, such as complex magnetism, unique charge transport, and superconductivity. Zintl A14MPn1...
  • 2026 - 09 - 02
    Click on the number of times: 2
    来源:ACS PublicationsEfficient and green separation of rare earth elements (REE) remains a critical challenge, with conventional solvent extraction relying heavily on toxic organic solvents. Herein, thr...
  • 2026 - 09 - 01
    Click on the number of times: 1
    来源:ACS PublicationsRare-earth activation in oxide thin films is often optimized empirically, although excitation-dependent upconversion (UC) is ultimately constrained by the near-surface energetic lan...
  • Copyright ©Copyright 2018 2020 Shanghai rare earth association All Rights Reserved Shanghai ICP NO.2020034223
    the host:Shanghai Association of Rare Earth the guide:Shanghai Development and Application Office of Rare Earth the organizer:Shanghai rare earth industry promotion center
    犀牛云提供云计算服务