Rare earth recycler draws $28 million in federal funding

The date of: 2020-09-16
viewed: 37

source:resource recycling

Urban Mining Co., which uses an innovative process to recycle rare earth magnets, has received financial backing as part of the U.S. response to the coronavirus pandemic.

San Marcos, Texas-based Urban Mining Co. operates a magnet recovery facility that’s about 130,000 square feet in size just south of Austin.

The company employs a magnet-to-magnet method to recycle the neodymium iron boron magnets (referred to as NdFeB magnets) used in hard disk drives, audio equipment and some industrial equipment.

The U.S. Department of Defense recently announced it will provide $28.8 million in funding to Urban Mining Co. through a Defense Production Act program. Called Title III, this program aims “to ensure the timely availability of essential domestic industrial resources to support national defense and homeland security requirements through the use of highly tailored economic incentives.”

In a release, the Department of Defense said the magnets recycled by Urban Mining Co. “are essential components for many [Department of Defense] programs that enable miniaturization and high performance of guidance, propulsion, and power systems.”

“This investment will enable Urban Mining Company to maintain and protect critical workforce capabilities during the disruption caused by COVID-19 while strengthening a vital domestic supply-chain of rare earth materials,” the federal agency continued.

Magnet use in growing number of sectors

The NdFeB magnets are frequently used in consumer electronics, which are a prime source of feedstock for Urban Mining Co. The company works with OEMs to receive devices through company takeback programs and sustainability initiatives, said Peter Afiuny, executive vice president of Urban Mining Co., in an interview.

But the magnets are increasingly being found in an array of industrial sectors, including energy, automotive, motion control and more.

“The overall demand is growing dramatically,” Afiuny said, noting that these additional sectors are “now surpassing the growth we’re seeing in consumer electronics.”

Afiuny said his company is differentiated by its development of a new method for magnet recovery.

“Our breakthrough was that we created a dry powder metallurgical process,” Afiuny said.

As E-Scrap News previously reported, the process avoids chemically reducing or converting the material into pure elements for new magnet production. Instead, the magnet is demagnetized and broken down into a powder that contains both the magnet and rare earth elements. A blend of elements, which is proprietary, is mixed in and the mixture is re-magnetized and formed into a new magnet.

The company currently handles about 2,000 tons per year of NdFeB magnets, Afiuny explained. Its facility is located on 100 acres of land and has plans for future growth.

Afiuny said he was limited in sharing information about how the funding will be distributed, due to terms of the agreement. But he noted a major part of Urban Mining Co.’s mission is “to build products for medical devices and the medical industry.”

“We have a pipeline that supports that and we want to continue to grow that,” he said.



Hot News / Related to recommend
  • 2026 - 11 - 13
    Click on the number of times: 1
    来源:Nature CommunicationsQuantifying three-dimensional (3D) orientation is critical for understanding self-assembly and collective behavior in soft matter and biological systems. Moreover, orientationa...
  • 2026 - 11 - 12
    Click on the number of times: 1
    来源:Nature CommunicationsRecycling end-of-life (EoL) NdFeB magnets is critical for securing supply of rare-earth element neodymium in the low-carbon transition. We develop a molten salt electrolysis re...
  • 2026 - 11 - 11
    Click on the number of times: 3
    来源:Science DirectZrB2-SiC ceramic composites are susceptible to severe oxidation corrosion at 1700 ℃ in oxidizing atmospheres, owing to rapid B2O3 volatilization, ZrO2-transformation-induced cracking,...
  • 2026 - 11 - 11
    Click on the number of times: 3
    Process intensification of low-concentration magnesium sulfate leaching of ion-adsorption rare earth ores by pulsed microwave-assisted gradient injection来源:Science DirectRare earth elements (REEs), pa...
  • Copyright ©Copyright 2018 2020 Shanghai rare earth association All Rights Reserved Shanghai ICP NO.2020034223
    the host:Shanghai Association of Rare Earth the guide:Shanghai Development and Application Office of Rare Earth the organizer:Shanghai rare earth industry promotion center
    犀牛云提供云计算服务