Colloidal Synthesis of Monodisperse High-Entropy Rare-Earth Oxide Nanoplatelets

The date of: 2026-09-07
viewed: 3

来源:ACS Publications

High-entropy rare-earth oxides (HE-REOs) offer a broad compositional space for tuning defect chemistry, lattice distortion, and local atomic environments, yet their controlled synthesis as monodisperse and structurally well-defined nanostructures remains challenging. Here, we report a colloidal approach for the synthesis of solution-dispersible, single-crystalline HE-REO nanoplatelets. The ultrathin two-dimensional nanoplatelets adopt a trigonal REO lattice that supports homogeneous multication incorporation across ternary to denary HE-REO compositions, and a simultaneous multication nucleation and growth pathway is demonstrated. Atomic-resolution imaging, combined with binary-type intensity classification, enables assessment of local chemical ordering, and increasing configurational entropy drives the system from a nearly random local structure toward a heteroelement-dominated short-range ordered state. High-entropy design further facilitates the incorporation of chemically dissimilar nonrare-earth cations, expanding the accessible miscibility window of REO nanostructures. Our work establishes colloidal synthesis as both a versatile route to monodisperse high-entropy oxide nanostructures and a model platform for probing and understanding entropy-governed behavior and functionality in high-entropy materials.



Hot News / Related to recommend
  • 2026 - 10 - 09
    Click on the number of times: 0
    来源:ACS PublicationsThe integration of diverse electronic phenomena, such as magnetism and nontrivial topology, into a single low-dimensional system gives rise to unusual quantum effects. Here we combi...
  • 2026 - 10 - 09
    Click on the number of times: 0
    来源:ACS PublicationsRare-earth elements (REEs: La–Lu, Y, Sc) are critical to modern technology; however, their acquisition, purification, and separation from each other can be challenging, and current ...
  • 2026 - 10 - 08
    Click on the number of times: 0
    来源:ACS PublicationsThe synthesis of alkali-metal-free compounds [LnMe3]n is scrutinized using two distinct protocols. The donor-promoted cleavage of homoleptic tetramethylaluminate complexes Ln(AlMe4)...
  • 2026 - 09 - 30
    Click on the number of times: 0
    来源:ScienceDirectIn the in-situ leaching of ionic rare earth ores, ineffective through-flow induced by ore body heterogeneity and suboptimal rinsing strategies constrain both extraction efficiency and ...