Controlling Selectivity of Surface Electro-Precipitation (SEP)

The date of: 2025-06-16
viewed: 23

Controlling Selectivity of Surface Electro-Precipitation (SEP) in the Recovery of Rare Earth Elements (REE) from Aqueous Feedstocks

 

来源:ACS Publications

SEP is an emerging green separation technique for the recovery of REE and other valuable elements from unconventional feedstocks. Its industrial adoption requires comprehensive mechanistic knowledge of its selectivity for REE vs typical background cations to achieve the desired separation. To bridge this gap, we experimentally studied SEP of neodymium Nd in chloride, nitrate, and sulfate solutions, in the absence and presence of calcium, aluminum, iron, zinc, and cobalt. We found that SEP is nonselective in the mass-transfer regime. It becomes selective in the mixed regime, with higher purification factors for elements with larger gaps in precipitation pH. At the same potential and initial pH, the selectivity of SEP in the mixed regime is controlled by the current (OH– generation rate) and background ions. In the case of Fe, it additionally depends on the catalytic activity of the SEP cathode in the production of H2O2. We demonstrated for the first time that the in situ production of hydrogen peroxide in SEP can be used to selectively remove Fe from a multielement solution. The reported selectivity-recovery figures make SEP highly competitive, especially when its other advantages are factored in. The results of this study can be the basis for developing a suitable SEP-based strategy for preconcentrating REE and other valuable elements from diluted secondary resources.

this study aimed to expand the basic knowledge of the selectivity of SEP for REE vs common interfering background elements. Toward this objective, we study (i) the effect of potential on the rate-determining step of the Nd recovery by SEP, (ii) the effect of the background anion (Cl–, NO3–, and SO42–) on this step, (iii) selectivity of SEP for Nd in the presence of typical co-ions such as Ca, Fe, Al, Zn, and Co, and (iv) the capability of SEP in separating Fe, Al, Zn and Co one from another. Although real feedstocks have much more complex compositions, adapting SEP to them requires an initial feasibility assessment in simpler synthetic solutions, as well as a fundamental understanding of selectivity trends. Moreover, the speciation of elements in real feedstocks is highly sensitive to fluctuations in dissolved O2 and CO2 as well as bacterial contamination during storage and handling. Along with their complex composition, this variability makes it more challenging to reproduce and interpret the trends observed in real feedstocks than in freshly prepared synthetic solutions.




Hot News / Related to recommend
  • 2026 - 02 - 10
    Click on the number of times: 2
    Curcuma longa debranched starch assisted synthesis of cerium oxide nanoparticles and its antioxidant, anticancer, antimicrobial, and anti-biofilm activities 来源:X-MOLNowadays, there is a growing emphas...
  • 2026 - 02 - 09
    Click on the number of times: 2
    Trivalent rare-earth ions (RE3+) exhibit sharp 4f–4f transitions that are highly sensitive to dipole–dipole interactions (DDIs), yet the intrinsic short-range of DDIs restricts their application in lo...
  • 2026 - 02 - 06
    Click on the number of times: 3
    来源:ACS PublicationsTo better understand the interactions of rare earth elements (REE) with anaerobic microorganisms, we explored the proteome response of a Clostridium strain to europium (Eu) and its ...
  • 2026 - 02 - 06
    Click on the number of times: 3
    来源:ACS PublicationsThe development of high-performance deep-ultraviolet (deep-UV) second-order nonlinear optical (NLO) crystals that simultaneously combine noncentrosymmetric crystal structure, broad ...