China cutting rare earth output, unnerving global manufacturers

The date of: 2018-11-19
viewed: 46

Source:Japan Today

LONDON/HOUSTON

The Chinese government is limiting domestic production of rare earth minerals in the second half of the year, a move likely to crimp international exports and send prices for the critical materials higher, according to data from Adamas Intelligence.

China is by far the world's largest producer and consumer of rare earths, a group of 17 elements used to make electric vehicles and consumer electronics. The move is already forcing manufacturers to scour the globe for alternative supplies.

For the second half of 2018, China's quota for rare earth separation and smelting has been cut 36 percent, an attempt to better control the market, according to Adamas, a research firm that closely tracks the rare earths industry.

China's decision to limit domestic rare earth production to 45,000 tons for the second half of 2018 - announced in August and the lowest in more than five years - provides only enough supply for China's domestic buyers, according to Adamas.

The semi-annual quota had risen to 70,000 tons in the first half of 2018, 40 percent higher than the first half of 2017. But that move was largely seen by analysts and electronics manufacturers as a step to legitimize black market production, with Chinese manufacturing consuming most of that supply.

While China is likely to attend to its own needs before exporting, increased exports would require the country to draw on already-low inventories of neodymium (Nd), prasesodymium (Pr) and dysprosium (Dy), used in electric vehicle motors, said Ryan Castilloux of Adamas.

Prices for one key rare earth mineral, PrNd Oxide, could increase by 10 percent to 50 percent within the next 12 months, and is on track to double in price within next five years as demand outpaces supply, Castilloux said.

Chinese exports typically supply around 80 percent of the globe's rare earth needs, about 156,000 tons annually. Still, exports tend to oscillate wildly from month to month.

In September, for example, rare earth exports jumped 15 percent from August levels, despite slipping earlier in the year, according to Chinese government data.

The Chinese Ministry of Industry and Information Technology and the Ministry of Natural Resources did not respond to faxed requests for comment.

WTO FIGHT

China was accused in 2012 of manipulating rare earths exports after it put quotas on overseas shipments in 2010.

In 2012, the United States, the European Union and Japan filed a complaint with the World Trade Organization accusing China of slashing exports to hold down prices for its own manufacturers and to pressure global firms to move to China.

China lost the case in 2014 after the WTO rejected its appeal and it lifted the export quotas.

The U.S. military is worried about China's dominance of the rare earths market, calling it a "significant and growing risk," according to a Pentagon study released earlier this month.

"As they have this standoff with China, eventually they (the U.S.) will need to find alternate sources," said Helen Lau, a metals and mining analyst at Argonaut Securities in Hong Kong, referring to the trade dispute between China and the United States.

However, Lau indicated in a research note that the change in the quota was likely tied to the closures of illegal mines in Jiangxi province last month.

"We are not surprised at the quota cuts as China already started a crackdown on illegal mining in Jiangxi province that started in September," she wrote.

Meanwhile Japanese electronics maker Panasonic Corp told Reuters said it is moving to find fresh supply.

"We have been diversifying our procurement channels, building partnerships with our suppliers and working to reduce the use of rare earths," Panasonic said in a statement to Reuters.

Outside of China, Australia's Lynas Corp is the biggest producer of PrNd oxides and the second-largest globally. The company processes rare earth ores from Australia at a plant in Malaysia.

During the quarter that ended in September, PrNd production climbed to a record 1,579 tons, the company said in its results.

Chief Executive Amanda Lacaze said that demand from Japanese customers was "absolutely buoyant," in a call with analysts after the report.

Lynas's processing plant is under environmental review, raising some concerns that supply could be lost, but for now it remains running.

Overall, prices for rare earths in China have been falling, said Daniel Morgan an analyst with UBS in Sydney. PrNd alloy metal prices in China are selling at 406,000 yuan ($58,400) a ton, down 24 percent from a year ago, according to data from Shanghai Metals Markets.

"What the price is telling you, is that there isn't a supply constraint up to now," Morgan said.

Research into rare earth alternatives has come up largely empty, leaving manufacturers beholden to the specialized minerals just as demand for batteries for electric vehicles and other products that use the materials is soaring.

A typical Toyota Prius, for example, uses 25 kilograms of rare earths, compared to 1 kilogram in a typical combustion-engine vehicle.


Hot News / Related to recommend
  • 2026 - 11 - 09
    Click on the number of times: 0
    来源:ACS PublicationsRare-earth hybrid nitrate double perovskites (REHNDPs) have recently emerged as an intriguing subclass of functional materials, combining structural diversity with rich intrinsic op...
  • 2026 - 11 - 09
    Click on the number of times: 0
    来源:ACS PublicationsRare-earth orthophosphates, REPO4, are highly insulating materials in which localized 4f moments interact through a phosphate framework, providing a model system for weak cooperativ...
  • 2026 - 11 - 06
    Click on the number of times: 4
    来源:ACS PublicationsConventional single-atom alloying (SAA) effect is generally regarded as a design strategy modulating the surface properties of an alloy system between those of its individual elemen...
  • 2026 - 11 - 05
    Click on the number of times: 5
    A system-integrated framework for rare earth element recovery: Source-specific extraction strategies from geological deposits to high-value anthropogenic reservoirs来源:Science DirectRare earth elements...
  • Copyright ©Copyright 2018 2020 Shanghai rare earth association All Rights Reserved Shanghai ICP NO.2020034223
    the host:Shanghai Association of Rare Earth the guide:Shanghai Development and Application Office of Rare Earth the organizer:Shanghai rare earth industry promotion center
    犀牛云提供云计算服务