News News
Contact us
  • Customer service number:64321087
  • Commercial service telephone:13918059423
  • Technical service telephone:13918059423
  • Contact person: Mr. Cui 
  • Service email:shxtb@163.com
  • Address: room 107, building 8, no. 100, guilin road, xuhui district, Shanghai

Controlling Ligand Excimer Formation with Dipole Changes in Emissive Rare-EarthPhosphonic Acid Complexes

The date of: 2025-09-26
viewed: 59

来源 :ACS  Publications

The interactions between substituted arylvinyl phosphonic acid (AVPA) ligands within a Eu-AVPA complex are shown to influence the outcomes of excited state evolution after photoexcitation. Compared with unfunctionalized AVPAs, pairs of ligands functionalized with CF3 in the para position preassociate in the ground state of complexes with Eu3+ according to calculated geometry optimizations. The CF3-substituted AVPA complexes show evidence of red-shifted optical absorption and undergo more efficient excimer formation, as revealed by transient absorption spectroscopy. We rationalize this behavior through simulations of excited-state geometry optimizations that reveal evolution toward interligand phenyl–phenyl planarity for specific excited states. Emission from complexed Eu3+ after energy transfer from the ligand is found to be weaker with CF3 substitution, which we hypothesize is due to intracomplex, interligand aggregates with excimer-promoting geometries. These observations point to the need to consider ground-state geometries as well as dynamic excited-state processes to understand the flow of energy in rare earth coordination complexes.



Hot News / Related to recommend
  • 2026 - 11 - 09
    Click on the number of times: 0
    来源:ACS PublicationsRare-earth hybrid nitrate double perovskites (REHNDPs) have recently emerged as an intriguing subclass of functional materials, combining structural diversity with rich intrinsic op...
  • 2026 - 11 - 09
    Click on the number of times: 0
    来源:ACS PublicationsRare-earth orthophosphates, REPO4, are highly insulating materials in which localized 4f moments interact through a phosphate framework, providing a model system for weak cooperativ...
  • 2026 - 11 - 06
    Click on the number of times: 4
    来源:ACS PublicationsConventional single-atom alloying (SAA) effect is generally regarded as a design strategy modulating the surface properties of an alloy system between those of its individual elemen...
  • 2026 - 11 - 05
    Click on the number of times: 5
    A system-integrated framework for rare earth element recovery: Source-specific extraction strategies from geological deposits to high-value anthropogenic reservoirs来源:Science DirectRare earth elements...
  • Copyright ©Copyright 2018 2020 Shanghai rare earth association All Rights Reserved Shanghai ICP NO.2020034223
    the host:Shanghai Association of Rare Earth the guide:Shanghai Development and Application Office of Rare Earth the organizer:Shanghai rare earth industry promotion center
    犀牛云提供云计算服务