Deciphering the Microstructures and Electronic Properties of the YVO4Re (Re = Pr, Nd, and Tm) Crysta

The date of: 2025-09-08
viewed: 40

来源:ACS Publications

Rare-earth ion (Pr3+, Nd3+, and Tm3+)-doped yttrium vanadate (YVO4) crystals have aroused great research interest owing to their excellent laser performances. However, the microstructures, which underlie the optical properties of these crystals, are still unclear. In this paper, the stable crystal structures of the YVO4:Re (Re = Pr, Nd, and Tm) systems are predicted by using the crystal structure analysis by the particle swarm optimization (CALYPSO) structure search method. The unique tetragonal structures with the P4̅m2 (no. 115) space group for the YVO4:Re crystals are identified for the first time. It is found that the rare-earth ions (Pr3+, Nd3+, and Tm3+) can accurately occupy the Y3+ sites and successfully fuse into the YVO4 host crystals. The simulated X-ray diffraction (XRD) patterns of the YVO4 and YVO4:Re (Re = Pr, Nd, and Tm) are consistent with the experimental measurements, demonstrating the possibility and rationality of the predicted structures. Furthermore, we are motivated to clarify the electronic properties of the pure YVO4 and YVO4:Re (Re = Pr, Nd, and Tm) crystals based on density functional theory (DFT). The calculated electronic band structures of YVO4:Re (Re = Pr, Nd, and Tm) indicate reductions in the band gaps. With the increase in f-electrons, the energies of the f-electrons in the conduction bands decrease slightly. The calculated electron localization functions (ELF) of YVO4:Re (Re = Pr, Nd, and Tm) show that the bonding characteristics of Y–O, Pr–O, Nd–O, and Tm–O are all ionic. These theoretical results could provide important information for further research on the rare-earth-doped laser materials.




Hot News / Related to recommend
  • 2026 - 07 - 17
    Click on the number of times: 0
    Hybrid Solvation Model for Analyzing the Binding of Yttrium and Calcium Cations to the Lanmodulin Protein Using the Fragment Molecular Orbital Method 来源:ACS PublicationsA hybrid solvation model combin...
  • 2026 - 07 - 16
    Click on the number of times: 0
    来源:ACS PublicationsChemically flexible A2B2O7 oxides are attractive candidates for designing structure-specific functional materials by judicious substitution. However, modulating functionality by sub...
  • 2026 - 07 - 16
    Click on the number of times: 0
    来源:ACS PublicationsRational design of Eu2+-activated red phosphors under visible light excitation remains a critical challenge in various fields such as photonics, optoelectronics, and white-light-emi...
  • 2026 - 07 - 15
    Click on the number of times: 0
    来源:ACS PublicationsPolaron formation has emerged as an important mechanism for unconventional luminescence in metal halide semiconductors. Here, we show that incomplete rare-earth-ion doping in the ze...