China raises annual rare earth output quotas to record high

The date of: 2019-11-11
viewed: 27

source:Reuters

* Mining quota at 132,000 T, smelting and separation at 127,000 T

* Annual quotas for 2019 are highest volumes ever allocated

* Beijing had raised prospect of limiting supply in U.S. trade row

* Quotas have been released unusually late in the year (Adds analyst and association official comment, milestone)

By Tom Daly

BEIJING, Nov 8 (Reuters) - China lifted its annual rare earth output quotas on Friday by 10% to record-high levels for 2019, potentially easing fears the world’s dominant producer of the group of 17 prized minerals will restrict supply.

Beijing in late May raised the prospect of weaponising its control of rare earths, used in everything from consumer electronics to sophisticated military equipment, in its trade war with the United States but has yet to announce any formal restrictions.

China is home to at least 85% of global rare earth processing capacity, according to Adamas Intelligence.

The full-year rare earth mining quota has been set at 132,000 tonnes for 2019 and the smelting and separation quota at 127,000 tonnes, the Ministry of Industry and Information Technology said in a statement.

ADVERTISEMENT

The quotas, up from 120,000 tonnes and 115,000 tonnes, respectively, in 2018, are the “highest volume ever allocated” David Merriman, a London-based manager at commodity research firm Roskill, said in an email.

China has now increased the allowances for two years in a row and an official at the Association of China Rare Earth Industry confirmed the numbers were record highs.

They imply a quota of 72,000 tonnes for mining in the second half of 2019, up more than 54% from an unusually low level a year earlier.

For smelting and separation, or the processing of ore into material manufacturers can use, the second half quota is 69,500 tonnes.

The quota hikes could be seen as a message that China has “the capability to increase supply, making life difficult for (rare earths) under development in regions such as the Americas, EU and Australia,” Roskill’s Merriman said.

But it likely “has much more to do with the domestic Chinese supply-chain situation,” he added, noting that China had been increasingly looking overseas for feedstock amid an environmental crackdown at home.

The move will allow state-run miners and processors to “legally maintain market share,” Merriman said.

China typically issues the rare earth quotas twice a year for six-month periods. In March, the first-half quotas were set at 60,000 tonnes for mining and 57,500 tonnes for smelting and separation.

ADVERTISEMENT

The late release of the full-year quotas comes as Beijing and Washington work to iron out the details on a so-called “phase one” deal to end trade hostilities.

China’s rare earth exports in October rose by 1.9% from the previous month to 3,639 tonnes, according to customs data released earlier on Friday. (Reporting by Tom Daly; Editing by Louise Heavens and Susan Fenton)



Hot News / Related to recommend
  • 2026 - 11 - 09
    Click on the number of times: 0
    来源:ACS PublicationsRare-earth hybrid nitrate double perovskites (REHNDPs) have recently emerged as an intriguing subclass of functional materials, combining structural diversity with rich intrinsic op...
  • 2026 - 11 - 09
    Click on the number of times: 0
    来源:ACS PublicationsRare-earth orthophosphates, REPO4, are highly insulating materials in which localized 4f moments interact through a phosphate framework, providing a model system for weak cooperativ...
  • 2026 - 11 - 06
    Click on the number of times: 4
    来源:ACS PublicationsConventional single-atom alloying (SAA) effect is generally regarded as a design strategy modulating the surface properties of an alloy system between those of its individual elemen...
  • 2026 - 11 - 05
    Click on the number of times: 5
    A system-integrated framework for rare earth element recovery: Source-specific extraction strategies from geological deposits to high-value anthropogenic reservoirs来源:Science DirectRare earth elements...
  • Copyright ©Copyright 2018 2020 Shanghai rare earth association All Rights Reserved Shanghai ICP NO.2020034223
    the host:Shanghai Association of Rare Earth the guide:Shanghai Development and Application Office of Rare Earth the organizer:Shanghai rare earth industry promotion center
    犀牛云提供云计算服务