High grade rare earths for Northern in Kimberley

The date of: 2019-08-22
viewed: 42

source:The West Australian

ASX-listed heavy rare earths producer Northern Minerals has intersected wide, high-grade rare earth element mineralisation from diamond drilling at both the Dazzler and Iceman prospects, part of its Browns Range operation near Halls Creek, WA.

The exceptional new results included 16.59 metres grading 7.53% total rare earth oxides, or “TREO”, from 27m down-hole and 18.6m @ 5.83% TREO from 25.4m in separate drill holes from Dazzler and 4.43m @ 8.07% TREO from 21m at Iceman.

Management said the grades were some of the highest returned from Browns Range and up to 10 times the total mineral resource grade currently being mined from the operation , 15km to the north.

A lower-grade zone of 10.3m @ 0.55% TREO from 48m down-hole was also recorded from Dazzler, which is more in line with the grades of the company’s Wolverine and Gambit West deposits and hosted in the same rock sequence as those ore bodies.

The company is now poised to wrap an updated mineral resource estimate around the Dazzler prospect later this quarter.

In March, Northern Minerals knocked out an impressive high-grade resource estimate at Dazzler totalling 144,000 tonnes grading 2.23% TREO, which is three times the average mined grade at Browns Range.

The high-grade zone at Dazzler is associated with a sedimentary unit close to a contact between sandstone and metamorphic rocks, whilst the low-grade zone was entirely within the footwall metamorphic sequence.

Northern said that the high-grade mineralisation at the Dazzler and Iceman prospects makes for an attractive target for the company, with such satellite deposits potentially acting as significant sweeteners to the more modest grades being extracted from Browns Range.

As with Browns Range, Dazzler and Iceman contain significant quantities of the sought-after element dysprosium, which is a key material utilised in making permanent industrial magnets used in the motors of electric vehicles amongst other applications.

The company is sitting on significant land holdings straddling this region near in the WA – Northern Territory boundary, which is underexplored by 21st Century standards.

Northern Minerals Managing Director George Bauk said:“ The grades returned in this program are amongst the highest we have ever seen at Browns Range.”

“We have already commenced the process of acquiring and installing Steinert ore sorting technology at Browns Range, aimed at doubling the feed grade to the plant.”

“The extremely high grades at Dazzler and Iceman have the potential to increase the grade going into the plant even further.”

“As with all resources projects, ‘grade is king’ and we look forward to increasing the value of Browns Range.”

Meanwhile, rare earth carbonate production continues at the company’s pilot plant project at Browns Range, which kicked off in earnest in July 2018.

The success of the operational flowsheet being employed to process the Browns Range mineralisation hosted by the mineral xenotime, has given Northern Minerals confidence that it will also potentially be able to treat the higher-grade Dazzler and Iceman rare earth ore materials in the future.

The regional deposits lie near the scarp of a 20m high range and hence their geometry is considered suitable for extraction using conventional open pit mining methods, if economic to do so.



Hot News / Related to recommend
  • 2026 - 09 - 18
    Click on the number of times: 1
    Solar Evaporation-Induced Mass-Transfer Enhancement in a Biomass-Derived Dual-Network Aerogel for Selective Enrichment of Rare-Earth Ions 来源:ACS PublicationsLow-concentration rare-earth industrial was...
  • 2026 - 09 - 17
    Click on the number of times: 3
    来源:ACS PublicationsCoal fly ash (CFA) represents a promising secondary source of rare-earth elements (REEs), yet their entrapment within the aluminosilicate glass matrix makes extraction difficult. He...
  • 2026 - 09 - 17
    Click on the number of times: 2
    来源:ACS PublicationsRare earth oxide phosphates (oxyphosphates), with extended metal-oxygen-phosphate bonding networks and a high rare-earth metal-to-phosphorus ratio (RE/P 1), are promising materials...
  • 2026 - 09 - 16
    Click on the number of times: 1
    来源:ACS PublicationsSurface plasmons modulate rare-earth luminescence via local field enhancement and photothermal effects, yet the synergy-competition between these inherently coupled effects remains ...
  • Copyright ©Copyright 2018 2020 Shanghai rare earth association All Rights Reserved Shanghai ICP NO.2020034223
    the host:Shanghai Association of Rare Earth the guide:Shanghai Development and Application Office of Rare Earth the organizer:Shanghai rare earth industry promotion center
    犀牛云提供云计算服务