Malaysia tells Lynas to remove rare earths radioactive waste

The date of: 2018-12-05
viewed: 49

Source:Aljazeera

Malaysia has told Lynas, the Australian company operating a rare earth elements processing plant on the country's east coast, that it must remove the radioactive waste that accumulated as a result of its activities over the past six years if it wants to continue to operate.

The decision on Tuesday follows a review of Lynas operations in Malaysia that was initiated by the government that took power in May's general election.

The "management of the waste residue from the Lynas Advanced Materials Plant (LAMP) should be given priority to ensure the wellbeing of the community and the environment", the Ministry of Energy, Science, Technology, Environment and Climate Change said in a statement.

The residue, some of it radioactive, has been building up at an open landfill at the Lynas site near the city of Kuantan since the processing plant started operations in 2012.

"The Ministry is concerned with the increasing risk of arising from the continued accumulation of residue without a viable solution to manage its accumulation in the near-term," the statement continued.

"For this reason, the Ministry will not allow the unlimited accumulation of residue at LAMP. The accumulated Water Leached Purification (WLP) Residue, which contains radioactive materials must be removed from Malaysia."

Radioactive waste

While Lynas was considering recycling the waste as a soil conditioner, the ministry said the duration of the studies was too short to reach a conclusion on the plan's safety. It said the waste would need to be removed from Malaysia by September 2, 2019, when Lynas' temporary storage licence expires.

The decision is likely to come as a blow to Lynas. The Australian-listed company had been campaigning hard to convince the review committee, government and the public that the plant was safe. It employs 600 people at the site.

The company said it was too early to comment. "We will release a statement once we have reviewed the report," it told Al Jazeera.

Lynas had previously said that the processing facility was run on a philosophy of "zero harm", urging "fairness, objectivity and transparency" in the review.

Rare earths are a crucial component in many of today's gadgets, including mobile phones, televisions and cars, but there are only a handful of producers around the world.

Malaysia's decision could have international ramifications, especially since China has already moved to limit domestic rare earths production in the second half of this year.

'Rational recommendation' 

Lynas' plant has been controversial from the start, triggering protests by activists and local residents concerned about the effect on public health and the environment.

They welcomed the government's decision.

"I would say the review committee has assessed the situation correctly," said Tan Bun Teet, chairman of Save Malaysia, Stop Lynas, which has campaigned against the plant since the beginning.

"They have made a very rational recommendation. For a corporation such as Lynas, operating on a huge scale and producing a large amount of waste, it's only pertinent that they have a workable and viable plan to manage waste safely."

The previous government awarded Lynas a temporary operating licence despite the public unease, but the company agreed it would "if necessary, remove from Malaysia all waste generated by the Lynas Advance Material Plant during the temporary operating licence's period".

The site currently has WLP residues totalling 451,564 metric tonnes and neutralisation underflow residue (NUF) of 1.113 million metric tonnes, the government said.

WLP is solid waste that contains natural-occurring radioactive material of 6.2 becquerels per gram that Malaysia required to regulate under the Atomic Energy Licensing Act 1984 because its radioactivity exceeds 1bq/g.


Hot News / Related to recommend
  • 2026 - 11 - 13
    Click on the number of times: 0
    来源:Nature CommunicationsQuantifying three-dimensional (3D) orientation is critical for understanding self-assembly and collective behavior in soft matter and biological systems. Moreover, orientationa...
  • 2026 - 11 - 12
    Click on the number of times: 0
    来源:Nature CommunicationsRecycling end-of-life (EoL) NdFeB magnets is critical for securing supply of rare-earth element neodymium in the low-carbon transition. We develop a molten salt electrolysis re...
  • 2026 - 11 - 11
    Click on the number of times: 3
    来源:Science DirectZrB2-SiC ceramic composites are susceptible to severe oxidation corrosion at 1700 ℃ in oxidizing atmospheres, owing to rapid B2O3 volatilization, ZrO2-transformation-induced cracking,...
  • 2026 - 11 - 11
    Click on the number of times: 2
    Process intensification of low-concentration magnesium sulfate leaching of ion-adsorption rare earth ores by pulsed microwave-assisted gradient injection来源:Science DirectRare earth elements (REEs), pa...
  • Copyright ©Copyright 2018 2020 Shanghai rare earth association All Rights Reserved Shanghai ICP NO.2020034223
    the host:Shanghai Association of Rare Earth the guide:Shanghai Development and Application Office of Rare Earth the organizer:Shanghai rare earth industry promotion center
    犀牛云提供云计算服务