来源:Nature Communications
Efficient 1.54 µm electroluminescence from erbium ions has long been hindered by their intrinsically small absorption cross-section and low excitation efficiency in conventional hosts. This study addresses the problem by synthesizing lead-free Cs3CrBr6 perovskite nanocrystals, a direct-bandgap n-type chromium-based halide semiconductor whose electronic structure affords good charge transport and makes it a suitable host for lanthanide doping. Er³⁺ incorporation acts as an efficient luminescent center while also modulating the host band structure. By exploiting the broadband absorption of Cr³⁺ for sensitization together with surface passivation, the authors achieve highly efficient Cr³⁺-to-Er³⁺ energy transfer, yielding intense 1.54 µm emission with a photoluminescence quantum yield of 47%. The corresponding electroluminescent device reaches a peak external quantum efficiency of 3.26%, among the highest reported for solution-processed Er³⁺-based near-infrared LEDs, validating the host's effectiveness in facilitating charge injection and transport. The work provides a viable material strategy for high-performance 1.54 µm emission and lays a foundation for chromium-based halide perovskites in advanced optoelectronics.