Exogenous organic acids drive efficient bioleaching of rare earth tailings by Acidithiobacillus thiooxidans

The date of: 2026-11-10
viewed: 2

Exogenous organic acids drive efficient bioleaching of rare earth tailings by Acidithiobacillus thiooxidans: Process optimization and interfacial mechanism

 

来源:Science Direct

The green recovery of rare earth elements (REEs) from rare earth tailings is crucial for resource recycling and mine ecological remediation. To address the low REEs leaching efficiency of a single Acidithiobacillus thiooxidans strain, this study evaluated the combined regulatory effects of four exogenous organic acids on REEs bioleaching, and elucidated the mechanisms via multiscale characterization and CatBoost machine learning model. The results showed that gluconic acid markedly enhanced REE leaching, raising the 8 day extraction efficiencies of La, Dy, and Y by 6.7–45%, 4–41%, and 12–32%, respectively, relative to the control across the tested dosages. Acetic acid exhibited an obvious inhibitory effect on leaching. Oxalic acid and citric acid showed concentration-dependent promotional effects with obvious threshold characteristics. XPS and BET analyses confirmed that the leaching system underwent dynamic structural evolution, and the complexation of organic acids with REEs and the surface coating of microbial extracellular polymers jointly regulated the leaching process. Pearson correlation and CatBoost model (R2=0.985) further revealed the intrinsic relationship between organic acid concentration, reaction time and leaching efficiency, providing theoretical support and technical reference for the green and efficient recovery of REEs from tailings.


Hot News / Related to recommend
  • 2026 - 11 - 13
    Click on the number of times: 0
    来源:Nature CommunicationsQuantifying three-dimensional (3D) orientation is critical for understanding self-assembly and collective behavior in soft matter and biological systems. Moreover, orientationa...
  • 2026 - 11 - 12
    Click on the number of times: 0
    来源:Nature CommunicationsRecycling end-of-life (EoL) NdFeB magnets is critical for securing supply of rare-earth element neodymium in the low-carbon transition. We develop a molten salt electrolysis re...
  • 2026 - 11 - 11
    Click on the number of times: 3
    来源:Science DirectZrB2-SiC ceramic composites are susceptible to severe oxidation corrosion at 1700 ℃ in oxidizing atmospheres, owing to rapid B2O3 volatilization, ZrO2-transformation-induced cracking,...
  • 2026 - 11 - 11
    Click on the number of times: 2
    Process intensification of low-concentration magnesium sulfate leaching of ion-adsorption rare earth ores by pulsed microwave-assisted gradient injection来源:Science DirectRare earth elements (REEs), pa...