Rare Earth-Silver Synergistic Strategy: Preparation of a Potential Antibacterial Material for Wound Related Applications

The date of: 2026-09-22
viewed: 8

来源:ACS Publications

Skin wounds usually cause delayed wound healing or infection due to the invasion of microorganisms, which seriously endangers human life and health. In the process of first aid and treatment, antibacterial dressings are usually used to achieve high efficiency in inhibiting infection and promoting wound healing. However, because of the widespread use of antibiotics or low-activity antibacterial ingredients in dressing fillers, research on dressing fillers is imminent. Here, we propose a preparation method for a high-performance dressing filler based on Y-based MOFs. Ag+ was adsorbed into the activation cavity of MOF-76-Y by supramolecular interactions and then reduced to zero-valent silver to anchor it in the framework structure of MOF-76-Y to prepare stable Ag@MOF-76-Y. Antibacterial evaluation of the system showed that Ag@MOF-76-Y has a high inhibition rate of 99.1% on Staphylococcus aureus, which is significantly higher than the antibacterial activity of MOF-76-Y. Further studies showed that its mild ROS generation rate, excellent bacterial removal efficiency, and excellent antibacterial activity were attributed to the host–guest synergy between Y-based MOFs and Ag. This work provides a new antibiotic-free, low-toxicity candidate for antibacterial dressing filler, promotes the development of next-generation dressings, and expands the application of rare earth compounds.


Hot News / Related to recommend
  • 2026 - 11 - 20
    Click on the number of times: 3
    来源:Nature CommunicationsEfficient 1.54 µm electroluminescence from erbium ions has long been hindered by their intrinsically small absorption cross-section and low excitation efficiency in conven...
  • 2026 - 11 - 19
    Click on the number of times: 4
    来源:Nature CommunicationsDry reforming of methane (DRM) with carbon dioxide produces CO-rich syngas for methanol and Fischer–Tropsch fuel synthesis, but carbon deposition deactivates catalysts and limi...
  • 2026 - 11 - 18
    Click on the number of times: 5
    来源:Nature CommunicationsSpatial-light computing requires rewritable, multilevel and persistent optical weights, but many implementations rely on volatile modulators or static power. Here we report a C...
  • 2026 - 11 - 17
    Click on the number of times: 8
    来源:Nature CommunicationsLanthanide-doped upconversion nanoparticles exhibit multicolor emission through discrete, narrowband transitions, enabling applications in bioimaging, lasers, and displays. How...