Synergistic Doping and Stabilization of Magnetically Tunable LnTi3(Sb,Sn)4 (Ln: Ce–Gd) Kagome Metals

The date of: 2026-07-24
viewed: 8

来源:ACS Publications

Here, we present our synthesis and characterization of the LnTi3(Sb,Sn)4 (Ln: Ce, Pr, Nd, Sm, Gd) family of cleavable kagome metals. While these materials are isostructural to the LnTi3Bi4 family, they only form as (Sb,Sn) solid-solutions with no corresponding LnTi3Sb4 or LnTi3Sn4 phases. We use a combination of first-principles density functional theory (DFT) and crystal orbital Hamilton population (COHP) calculations to show that (Sb,Sn) alloying has a stabilizing effect on the structure by adjusting the Fermi level, filling bonding states, depopulating antibonding states, and adjusting the density of states (DOS) toward local minima, an effect we call “synergistic doping.” Through a detailed characterization of the SmTi3(Sb,Sn)4 series, we further demonstrate that the tunable Fermi level has a profound effect on the physical properties. We observe multiple magnetic phases that stem from a competition between antiferromagnetic (AFM) and ferromagnetic-like (FM) ground states. Furthermore, the (Sb,Sn) ratio allows us to tune from direct AFM-FM competition toward a complex admixture with properties reminiscent of the recently discovered TbTi3Bi4. Ultimately, our work demonstrates how the concept of synergistic doping provides a means to stabilize new structures while developing systems with intrinsically tunable chemical, magnetic, and electronic properties.



Hot News / Related to recommend
  • 2026 - 09 - 21
    Click on the number of times: 0
    来源: ACS PublicationsThe effects and mechanisms of preconception couples’ coexposure to rare earth elements (REEs)─emerging reproductive toxicants─on spontaneous abortion (SA) remain unclear. This nest...
  • 2026 - 09 - 21
    Click on the number of times: 0
    来源:ACS PublicationsMonodisperse oxide nanoparticles have attracted attention for biomedical applications. However, conventional synthetic methods often provide limited control over particle size, morp...
  • 2026 - 09 - 18
    Click on the number of times: 1
    Solar Evaporation-Induced Mass-Transfer Enhancement in a Biomass-Derived Dual-Network Aerogel for Selective Enrichment of Rare-Earth Ions 来源:ACS PublicationsLow-concentration rare-earth industrial was...
  • 2026 - 09 - 17
    Click on the number of times: 4
    来源:ACS PublicationsCoal fly ash (CFA) represents a promising secondary source of rare-earth elements (REEs), yet their entrapment within the aluminosilicate glass matrix makes extraction difficult. He...