Eu2Li(C3)H: A Carbide Hydride Phase Incorporating Eu2+

The date of: 2026-01-16
viewed: 20

来源:ACS Publications

Reactions between carbon and lithium hydride in a mixed metal europium/lithium flux led to the synthesis of Eu2Li(C3)H. At room temperature, the compound crystallizes in the tetragonal space group P4/mbm (no. 127, Z = 2; Ca2Li(C3)H type) and undergoes a second-order structural phase transition below ∼250 K to an orthorhombic low-temperature modification (no. 55, Pbam; Z = 4), crystallizing in a new structure type. The phase transition was monitored by using single-crystal X-ray diffraction (SCXRD) and temperature-dependent high-resolution powder diffraction data. Infrared (IR) spectroscopy and gaschromatographic analysis (GC) of the hydrolysis products confirm the existence of a first europium compound with an allylenide anion (C34–). Magnetic susceptibility measurements and 151Eu Mössbauer spectroscopy reveal the presence of divalent europium, suggesting a charge-balanced carbide hydride (Eu2+)2(Li+)(C34–)(H–). A transition to a (soft) ferromagnetic ground state is observed below 42 K. In situ high-pressure, high-temperature (HPHT) investigations indicate a surprisingly high stability of Eu2Li(C3)H and yield a bulk modulus K0 = 65 GPa. Quantum chemical calculations (DFT + U) reveal a pseudogap at the Fermi level and allow the classification as a rare-earth metal Zintl phase exhibiting both ionic and covalent bonding contributions.


Hot News / Related to recommend
  • 2026 - 07 - 30
    Click on the number of times: 4
    来源:ACS PublicationsHeterobimetallic rare-earth-nickel alkyl complexes (RE-Ni-alkyl) supported by an arene-anchored bis(phosphinomethylamido) ligand were synthesized and further reacted with MesPH2 (Me...
  • 2026 - 07 - 30
    Click on the number of times: 4
    来源:ACS PublicationsRare earth elements (REEs) are essential for contemporary technologies; however, their sustainable recovery from aqueous media remains challenging due to limited reserves and the en...
  • 2026 - 07 - 28
    Click on the number of times: 4
    来源:ACS PublicationsThe molten flux method was used to grow crystals belonging to two different classes of rare-earth hafnium molybdates, RE2Hf3(MoO4)9 and RE2Hf2(MoO4)7, whose luminescence and magneti...
  • 2026 - 07 - 28
    Click on the number of times: 5
    来源:ACS PublicationsRecovering rare earth (RE) ions from mining wastewater offers several advantages, including reducing resource scarcity, minimizing environmental pollution, and lowering biological t...
  • Copyright ©Copyright 2018 2020 Shanghai rare earth association All Rights Reserved Shanghai ICP NO.2020034223
    the host:Shanghai Association of Rare Earth the guide:Shanghai Development and Application Office of Rare Earth the organizer:Shanghai rare earth industry promotion center
    犀牛云提供云计算服务