Inverse-Sandwich Rare Earth Metal Complexes Comprising a Planar Toluene Dianion

The date of: 2026-01-06
viewed: 29

来源:ACS Publications

We report the first inverse-sandwich complexes containing rare earth (REIII) metal ions that captured a toluene dianion between them. Toluene-bridged complexes [{(Me3Si)2NC(NiPr)2}2RE]2(μ-η6:η6-C6H5Me) (RE = Y (1), Dy (2), and Er (3)) were synthesized via chemical reductions of chloride-bridged RE complexes in which each tripositive metal is stabilized by two guanidinate ligands. Compounds 1–3 were unambiguously characterized by crystallography, NMR, UV–vis, and IR spectroscopy, magnetometry, and computations. The bond metrics from single-crystal X-ray diffraction analysis revealed a planar, cyclohexadienediide-like structure for the ligated arene, indicative of a dianionic toluene. The 1H NMR spectrum of 1 exhibits upfield-shifted resonances representing increased shielding from excess electrons, further validating its dianionic nature. DFT calculations afforded similar bond metrics, and natural bond orbital (NBO) analysis uncovered ionic bonding interactions between the bridging toluene and the yttrium centers, supporting the assignment of a −2 charge to the toluene. UV–vis spectroscopy highlighted that the electronic excitations primarily stem from toluene- and guanidinate-based orbitals. The Dy and Er congeners were further probed by SQUID magnetometry, with 3 revealing weak magnetic exchange coupling between the ErIII centers. These findings highlight the ability of reduced arenes to serve as bridging ligands in multimetallic rare earth architectures.



Hot News / Related to recommend
  • 2026 - 09 - 21
    Click on the number of times: 2
    来源: ACS PublicationsThe effects and mechanisms of preconception couples’ coexposure to rare earth elements (REEs)─emerging reproductive toxicants─on spontaneous abortion (SA) remain unclear. This nest...
  • 2026 - 09 - 21
    Click on the number of times: 0
    来源:ACS PublicationsMonodisperse oxide nanoparticles have attracted attention for biomedical applications. However, conventional synthetic methods often provide limited control over particle size, morp...
  • 2026 - 09 - 18
    Click on the number of times: 1
    Solar Evaporation-Induced Mass-Transfer Enhancement in a Biomass-Derived Dual-Network Aerogel for Selective Enrichment of Rare-Earth Ions 来源:ACS PublicationsLow-concentration rare-earth industrial was...
  • 2026 - 09 - 17
    Click on the number of times: 4
    来源:ACS PublicationsCoal fly ash (CFA) represents a promising secondary source of rare-earth elements (REEs), yet their entrapment within the aluminosilicate glass matrix makes extraction difficult. He...