Development of rare earth element-based hybrid aluminium composites using stir casting process

The date of: 2024-11-15
viewed: 36
source:Scientific Reports


Abstract
Aerospace and marine industries are constantly in search of materials that can provide good strength and durability while also being lightweight. Aluminium composites with adequate reinforcements have been proven to be effective in achieving incredible mechanical properties while also maintaining a good strength to weight ratio. Numerous studies have been done to study the various possibilities of matrix reinforcement combinations in aluminium composites. This work focuses on studying the effect of varying Cerium Oxide (CeO2) percentage in the aluminium composite on its tensile strength, hardness and corrosion resistance. CeO2 is used along with Silicon Carbide (SiC) and Multi-Walled Carbon Nanotubes (MWCNT) to develop four samples of hybrid aluminium composites with SiC and MWCNT constituting 1% and 0.1% of the composite and the weight percentage of CeO2 is varied between 1 and 2.5%. All the samples were fabricated using the modified stir casting process. The results show that the hardness and tensile strength of the composites peak when the CeO2% is at 2% while corrosion resistance only gets better with increasing reinforcement content. A significant enhancement in mechanical and physical properties of aluminium composite suggests that MWCNT is an effective hybridizing agent with SiC and CeO2 to develop aluminium composites.



Hot News / Related to recommend
  • 2026 - 10 - 22
    Click on the number of times: 0
    Mechanisms of rare earth element and aluminum leaching with magnesium sulfate based on coupled seepage–chemical–diffusion simulations in microporous networks来源:Science DirectIn situ leaching of ionic ...
  • 2026 - 10 - 22
    Click on the number of times: 0
    来源:Science DirectRare-earth mono-nitrides (REN) are important rare-earth compounds whose structural stability and electronic structure are strongly influenced by localized 4f states. In this work, a f...
  • 2026 - 10 - 21
    Click on the number of times: 0
    来源: Science DirectThe reason for the higher extraction rate of light rare earth elements (LREY) than that of heavy rare earth elements (HREY) during the extraction of rare earth elements (REY) from co...
  • 2026 - 10 - 20
    Click on the number of times: 0
    来源:ACS Publications High-quality single crystals of refractory oxides are essential for fundamental investigations and advanced functional characterization, yet their preparation is frequentl...
  • Copyright ©Copyright 2018 2020 Shanghai rare earth association All Rights Reserved Shanghai ICP NO.2020034223
    the host:Shanghai Association of Rare Earth the guide:Shanghai Development and Application Office of Rare Earth the organizer:Shanghai rare earth industry promotion center
    犀牛云提供云计算服务