New research unveils extreme complexity in formation of rare earth mineral vital for tech industry

The date of: 2024-05-21
viewed: 40
source:Trinity College Dublin


In a new study, researchers from Trinity have unveiled that myriad, intricate factors influence the genesis and chemistry of bastnäsite and rare earth carbonates, which are critically needed for today's tech industry and its hardware outputs.
Their work, published in the international journal Global Challenges, unveils a newly acquired depth of understanding that had previously been unexplored in this field. In combination, the findings mark a significant advancement and promise to reshape our understanding of rare earth mineral formation.
Crucially, as global demand for rare earth elements continues to rise—largely to satisfy the growing demand for the mobile phones, batteries and speakers in which they are put to work—insights from this research could have far-reaching implications and various industrial and environmental applications.
Contrary to prior assumptions, the new research reveals that the formation of bastnäsite—the top rare earth mineral exploited by industry—is not a straightforward process but instead one driven by a very complex interplay of multiple factors.
The experimental approach involved studying the interaction between solutions containing multiple rare earth elements and common calcium-magnesium carbonate minerals like calcite, aragonite and dolomite (which are ubiquitous in nature) under hydrothermal conditions ranging from 21°C to 210°C. The team tested two solution types: one with equal rare earths concentrations, and another one simulating concentrations more typical of the usual hydrothermal fluids found on Earth.
The findings show that when the common calcium-magnesium carbonate minerals react with rare earth-rich fluids, they change their structures and chemical compositions, forming a series of rare earth-bearing minerals with exotic names like lanthanite, kozoite, bastnasite and cerianite, with very complex chemistries, shapes and textures.
Particularly interesting is that different solution types lead to distinct outcomes: For example, equal-concentration solutions promote kozoite and bastnasite crystallization, maintaining similar rare earths ratios in solids and solutions.
Conversely, hydrothermal fluids mimicking the ones found on Earth result in rare earth-bearing minerals with varied elemental distributions—and some of these even go through decarbonation processes due to the formation of rare earth oxides.
Ultimately, the experiments showcase the extremely dynamic nature of rare earths mineral formation, with unstable minerals transforming into more stable ones over time, and sometimes developing textures impacted by adjacent mineral reactions that further underscore the complexity of the process.
The implications of this research extend far beyond the laboratory. Understanding the complex processes involved in bastnäsite formation has profound implications for geologists and industry alike. The research demonstrates that the development of advanced simulation models is strongly needed, allowing scientists to replicate natural conditions and explore alternative methods for mineral extraction or synthesis.
While challenges remain, the insights from this study open the door for new experimental protocols to understand the fate of rare earth elements in complex geological ores where they concentrate.
Melanie Maddin, Ph.D. Candidate in Geology in Trinity's School of Natural Sciences, is the lead author of this study. She said, "These findings challenge the models previously applied to rare earth mineral formation.
"Our research highlights the dependence of crystallization pathways, mineral formation kinetics, and chemical texture on a myriad of factors, including rare earth concentrations, ionic radii, temperature, time, and host grain solubility."
Juan Diego Rodriguez-Blanco, Principal Investigator of the research group and Professor in Trinity's School of Natural Sciences, emphasized the significance of these findings in understanding not only bastnäsite formation but also the broader field of rare earth mineralogy.
Dr. Rodriguez-Blanco, a funded investigator in iCRAG (Science Foundation Ireland Research Center in Applied Geosciences), said, "This study opens new avenues for research in geochemistry and mineralogy, paving the way for a more comprehensive understanding of mineral formation processes."



Hot News / Related to recommend
  • 2026 - 11 - 23
    Click on the number of times: 1
    来源:Communications MaterialsSilicon photonics is a solid candidate to address the challenges of emerging communication systems with an increasing number of interconnected devices. However, the properti...
  • 2026 - 11 - 20
    Click on the number of times: 9
    来源:Nature CommunicationsEfficient 1.54 µm electroluminescence from erbium ions has long been hindered by their intrinsically small absorption cross-section and low excitation efficiency in conven...
  • 2026 - 11 - 19
    Click on the number of times: 9
    来源:Nature CommunicationsDry reforming of methane (DRM) with carbon dioxide produces CO-rich syngas for methanol and Fischer–Tropsch fuel synthesis, but carbon deposition deactivates catalysts and limi...
  • 2026 - 11 - 18
    Click on the number of times: 10
    来源:Nature CommunicationsSpatial-light computing requires rewritable, multilevel and persistent optical weights, but many implementations rely on volatile modulators or static power. Here we report a C...
  • Copyright ©Copyright 2018 2020 Shanghai rare earth association All Rights Reserved Shanghai ICP NO.2020034223
    the host:Shanghai Association of Rare Earth the guide:Shanghai Development and Application Office of Rare Earth the organizer:Shanghai rare earth industry promotion center
    犀牛云提供云计算服务