This meteorite material could power our clean energy future

The date of: 2022-11-22
viewed: 32
source:freethink


By figuring out how to manufacture in the lab a rare mineral, previously found only in meteorites, two teams of researchers may have just helped secure America’s clean energy future. 
Permanent magnets: Of the 118 elements on the periodic table, 17 fall into the category of “rare earths,” and contrary to their name, these materials aren’t terribly rare — each is more common than gold, and one is more plentiful than even copper.
Rare earth elements are used to make a slew of products, from smartphone screens to x-ray machines, but permanent magnets are arguably the most important. 
These are objects that, once magnetized, create their own magnetic fields, and we need them to build wind turbines, EV motors, and other products that play a vital role in the battle against climate change.
A shaky supply: Rare earth elements may not be exactly “rare,” but because they are widely dispersed in the Earth’s crust, miners need to go through the environmentally destructive process of extracting, and processing, a lot of material to get a small amount of rare earths.
That hasn’t deterred China from tapping into its large supply of rare earth elements, though — the nation dominates the rare earth market and manufactures more than 90% of the world’s rare earth permanent magnets.
The mineral tetrataenite has magnetic properties that make it a leading contender for replacing traditional rare earth elements in permanent magnets. The problem is that it basically doesn’t naturally form on Earth — it’s found almost exclusively in meteorites, which cooled extremely slowly over millions of years.
What’s new? In October 2022, two different groups — one at Northeastern University and one at the University of Cambridge — announced that they’d figured out how to make tetrataenite in the lab.
They aren’t the first to manufacture the meteorite material, but unlike past techniques — which required scientists to expose iron-nickel alloys to radiation — their methods have the potential for mass production.
Two new techniques for making tetrataenite in the lab could lead to its mass production.
How it works: The Northeastern team found that it could manufacture tetrataenite by heating and cooling an iron-nickel alloy, while applying extensional stress and a magnetic field.
Cambridge’s technique, meanwhile, centers on the mixing of precise quantities of phosphorus with iron and nickel.
“What was so astonishing was that no special treatment was needed: we just melted the alloy, poured it into a mold, and we had tetrataenite,” said lead researcher Lindsay Greer. 
Looking ahead: Northeastern researcher Laura Lewis told NPR that her team still needs to test its tetrataenite to see if it holds up against the kind that comes from meteorites. Even if it does, it would be at least 5 to 8 years before it could be used to make permanent magnets.
The Cambridge team says it also needs to research whether its synthetic tetrataenite could be used to make permanent magnets — it hopes to suss that out with the help of major magnet manufacturers.
“We just melted the alloy, poured it into a mold, and we had tetrataenite.”
LINDSAY GREER
The big picture: If the US could manufacture its own tetrataenite, it could reduce our dependence on China for permanent magnets, but we’d still be reliant on Chinese supply chains for the rare earth elements needed to make other products.



Hot News / Related to recommend
  • 2026 - 10 - 30
    Click on the number of times: 0
    来源:Science DirectFluoride in ionic rare earth ore leachate readily induces three-phase emulsification during rare earth solvent-extraction process, severely worsening separation efficiency and product...
  • 2026 - 10 - 30
    Click on the number of times: 0
    来源:Science DirectProlonged MgSO4 in-situ leaching (ISL) of ion-adsorption rare earth element deposits may alter rare earth elements (REEs) vertical distribution, fractionation, and speciation, but fie...
  • 2026 - 10 - 29
    Click on the number of times: 0
    来源:ACS PublicationsTo ensure supply chain security, highly selective recovery of rare-earth elements (REEs) from industrial solid wastes is essential. In this study, UiO-66-NH2 was functionalized with...
  • 2026 - 10 - 28
    Click on the number of times: 0
    来源:ACS PublicationsRare earth elements, characterized by their partially filled 4f orbitals and exceptional electron transfer capabilities, play an irreplaceable regulatory role in both acid-base and ...
  • Copyright ©Copyright 2018 2020 Shanghai rare earth association All Rights Reserved Shanghai ICP NO.2020034223
    the host:Shanghai Association of Rare Earth the guide:Shanghai Development and Application Office of Rare Earth the organizer:Shanghai rare earth industry promotion center
    犀牛云提供云计算服务