Scientists invent material for neutrons and gamma-rays

The date of: 2021-12-27
viewed: 24

source:The News Motion


Dr. Huo Zhipeng and his student Zhao Sheng from the Hefei Institutes of physical science (HFIPS) of the Chinese Academy of Sciences recently developed a lead-free neutron and gamma ray composite shielding material that has high shielding properties and is environmentally friendly. Their results were published in Nuclear Materials and Energy.

The composite, modified-gadolinium oxide/boron carbide/high density polyethylene (Gd2O3/B4C/HDPE), was tested safe and effective to shield neutron and gamma rays through a series of intricate and comprehensive experiments.

Neutron, as an electrically neutral particle, has a strong penetrability and always emits secondary gamma rays during particle collision process. The scientific and efficient scheme of shielding neutron is to select high Z (atomic number), low Z materials, and neutron absorbing materials simultaneously for combined shielding. However, lead-containing materials are restricted in application with biological toxicity.

Rare earth element gadolinium, usually exists in the form of non-toxic Gd2O3 in nature, has always shown high average thermal neutron absorption, high temperature resistance and good gamma shielding performance.   

The researchers studied the shielding mechanism first, and then adopted the coupling agents to modify the surface of Gd2O3 to improve the interfacial compatibility and dispersion of Gd2O3 in the matrix.

“It is lead-free and poses no threat to the environment or humans,” said Dr. Huo, who has been engaged in radiation and environmental protection for years. 

He further explained how this radiation shielding system worked. Fast neutrons collide with gadolinium (Gd) inelastically, and collide elastically with hydrogen until they become thermal neutrons, finally, absorbed by high Z element Gd and boron.

The experimental results show that the neutron shielding rate of the composite can reach 98% under the condition of 15 cm thickness in CF-252 environment. In cS-137 and CO-60 environments, the gamma shielding rates of the composite are 72% and 60%, respectively, at the same thickness.   

Its comprehensive shielding performance is better than conventional boron-polyethylene collimating shielding, and it is suitable for neutron spectrum and gamma spectrum diagnosis system of Experimental Advanced Superconducting Tokamak (EAST). It is expected to be a promising radiation shielding material for neutron-gamma mixed fields, according to the researchers.



Hot News / Related to recommend
  • 2026 - 11 - 27
    Click on the number of times: 5
    来源:Scientific ReportsThis study presents a comprehensive investigation into the distribution and recovery of rare earth elements (REEs) throughout the phosphoric acid production process. Analysis of i...
  • 2026 - 11 - 26
    Click on the number of times: 6
    来源:Communications MaterialsIn A2BB'O6 double perovskites (DPs) containing 3d and 5d magnetic ions, the magnetic behavior of the B sublattice can be tuned by choosing nonmagnetic isovalent B' c...
  • 2026 - 11 - 25
    Click on the number of times: 10
    来源:Nature CommunicationsLanthanides serve as essential cofactors in the methanol dehydrogenases of methylotrophic bacteria. While biological function has been characterized for the naturally occurring...
  • 2026 - 11 - 24
    Click on the number of times: 6
    来源:Communications MaterialsConventional polymeric radiation shielding materials suffer from filler aggregation, weak interfacial bonding, and metal leaching. This work presents a chelation immobilizat...
  • Copyright ©Copyright 2018 2020 Shanghai rare earth association All Rights Reserved Shanghai ICP NO.2020034223
    the host:Shanghai Association of Rare Earth the guide:Shanghai Development and Application Office of Rare Earth the organizer:Shanghai rare earth industry promotion center
    犀牛云提供云计算服务