Potential Biosensor and Cancer Applications of Cerium Oxide Nanoparticles

The date of: 2021-12-08
viewed: 51

source:AZO NANO


A study recently published in the journal Nanomanufacturing examines the cytotoxicity and biocompatibility of cerium oxide (CeO2) nanoparticles for use in different applications such as fuel cells, cancer treatment, auto-exhaust catalysts, and biosensors.

Cerium oxide has received a lot of interest in recent years owing to its unique physical and chemical features. However, extensive use has resulted in their leakage into the ecosystem, where human exposure can cause serious health issues.

Cerium Oxide Nanoparticles: Formation & Applications

Cerium is a rare earth metal that combines with oxygen to produce cerium oxide nanoparticles with a crystalline structure. Cerium oxide nanoparticles exhibit excellent antioxidant characteristics because of the redox cycling between the two active states of cerium, 3+ and 4+.

Due to a large number of oxygen-containing functional groups in CeO2 nanoparticles, they can operate as an electrolyte in supercapacitors, as well as in nanomaterial applications such as fuel cells, rust inhibitors, and catalytic converters.

CeO2 nanoparticles are used for a wide variety of applications in the healthcare industry as well.

When tested against several types of bacteria, these rare earth nanoparticles (nanoceria) showed a significant antibacterial impact. In addition to their natural ability to change oxidation states, CeO2 nanoparticle can also protect healthy cells from oxidative damage.

Furthermore, cerium oxide nanoparticles can function as synthetic oxidative electrocatalysts with observable central nervous system (CNS) penetrance, sustained preservation, and restorative catalytic properties. 

Biosafety Concerns of Cerium Oxide Nanoparticles

Continuous, frequent use of these nanomaterials has resulted in their constant discharge into the atmosphere, where human exposure can cause severe health issues. Therefore, toxicity and biosafety evaluation are crucial before their widespread use in industrial applications increases. 

The published data on the toxicity and biosafety of cerium oxide nanoparticles is inconsistent. Several papers have commented on the low toxicity and anti-inflammatory properties of CeO2 nanoparticles.

On the other hand, harmful consequences of cerium oxide nanoparticles have also been described, including cell death. Harmful impacts were shown to be due to the formation of reactive oxygen species (ROS), which can induce cellular damage and eventually result in the initiation of cell death.

Interestingly, it has also been shown that cerium oxide nanoparticles display either antioxidant or pro-oxidative characteristics.

Research Methods

In this study, the researchers employed a hydroxide-mediated methodology to synthesis cerium oxide nanoparticles, and characterization techniques such as SEM, EDX, and XRD, among others, were employed to investigate their characteristics.

Live/Dead cell assays and Reactive Oxygen Species (ROS) assays were used to evaluate the toxicity and cytocompatibility of CeO2 nanoparticles.

A straightforward synthesis procedure was used. In a beaker, a 0.1 M cerium nitric acid solution was agitated, and a 0.3 M sodium hydroxide solution was poured into it. This mixture was then centrifuged for 15 minutes at 8000 revolutions per minute to get the sediment to settle at the bottom.

The cerium oxide nanoparticles were obtained by depositing the sediment on a glass plate and drying it in a warm air vacuum furnace at 200 degrees Celsius.

Research Findings

The cerium oxide nanoparticles were produced effectively using a hydroxide-treatment method, yielding pale-yellow nanostructures.

SEM established the crystal size to be in the range of 10 to 30 nm, and EDX confirmed the crystalline phase of the nanoparticles to be free of any extraneous contaminants.

The existence of cerium oxide nanoparticles was established using FTIR, whereas the crystalline composition of the nanoparticles was established by the XRD results.

Tests utilizing Beas-2B cells in the MTT, Live/Dead survivability, and ROS assays revealed that the cerium oxide nanoparticles are sustainable with the cells, with no cell damage even at very high concentrations.

Future Perspectives

The findings show that the cerium oxide nanoparticles can be employed in multiple medical applications, including biosensors and cancer treatment.

The filtration and absorption capabilities of CeO2 nanoparticles are useful for products like catalytic converters and sunblock. Cerium oxide nanoparticles can also be used for drug delivery because of their tiny size, which allows them to pass through cell membranes.



Hot News / Related to recommend
  • 2026 - 11 - 13
    Click on the number of times: 1
    来源:Nature CommunicationsQuantifying three-dimensional (3D) orientation is critical for understanding self-assembly and collective behavior in soft matter and biological systems. Moreover, orientationa...
  • 2026 - 11 - 12
    Click on the number of times: 1
    来源:Nature CommunicationsRecycling end-of-life (EoL) NdFeB magnets is critical for securing supply of rare-earth element neodymium in the low-carbon transition. We develop a molten salt electrolysis re...
  • 2026 - 11 - 11
    Click on the number of times: 3
    来源:Science DirectZrB2-SiC ceramic composites are susceptible to severe oxidation corrosion at 1700 ℃ in oxidizing atmospheres, owing to rapid B2O3 volatilization, ZrO2-transformation-induced cracking,...
  • 2026 - 11 - 11
    Click on the number of times: 2
    Process intensification of low-concentration magnesium sulfate leaching of ion-adsorption rare earth ores by pulsed microwave-assisted gradient injection来源:Science DirectRare earth elements (REEs), pa...
  • Copyright ©Copyright 2018 2020 Shanghai rare earth association All Rights Reserved Shanghai ICP NO.2020034223
    the host:Shanghai Association of Rare Earth the guide:Shanghai Development and Application Office of Rare Earth the organizer:Shanghai rare earth industry promotion center
    犀牛云提供云计算服务