来源:ACS PublicationsDiatomic catalysts (DACs) hold inherent superiority in atomic economy and synergistic catalysis for complex multi-intermediate reactions. However, several fundamental challenges persist, including typically low diatomic loading (2 wt %), ambiguous diatomic site identification, and most critically, the lack of universal design principles for rational synthesis. Herein, we present a general synthetic strategy guided by the hard–soft acid–base (HSAB) principle, successfully yielding 14 rare-earth (RE)-based DACs with record-high metal loadings (12.8–30.7 wt %, 3.2–5.4 at. %) an...
Release time:
2026
-
03
-
20
viewed:17
来源:ACS PublicationsCe-based polar materials are promising NLO candidates due to their unique electronic configuration of [Xe] 4f15d16s2 and diverse coordination modes. Ce4+ compounds are highly desired candidates for advanced nonlinear optical materials, yet the development of trivalent cerium-based NLO materials exhibiting a high second-harmonic-generation (SHG) response (above 3.0 × KDP) remains a great challenge. Herein, a new cerium iodate, Ce2(IO3)6(H2O), crystallized in the polar space group Pn (No. 7), was discovered by introducing rare-earth cations into iodates with a hydrotherma...
Release time:
2026
-
03
-
19
viewed:14
来源:ACS PublicationsThe integration of two-dimensional (2D) semiconductors into next-generation electronics critically depends on the availability of high-κ dielectrics that combine wide band gaps, strong breakdown fields, and pristine interfaces. Conventional oxides such as HfO2 suffer from interfacial incompatibility with 2D channels, while van der Waals dielectrics like h-BN offer excellent stability but limited capacitance. Here, we report the synthesis of quasi-vdW samarium oxybromide (SmOBr) nanosheets via a molten salt-assisted chemical vapor deposition method, establishing a previously ...
Release time:
2026
-
03
-
18
viewed:16
来源:ACS PublicationsWe report a novel Task-Specific Ionic Liquid (TSIL) derived from ciprofloxacin in combination with CYPHOS·NTf2 that enables tunable selectivity toward the extraction of rare earth metal elements (REEs), thorium, uranium, titanium, and zinc. The highest metal-TSIL affinity was found at pH 6, showing the highest extraction coefficient values for thorium (446), uranium (404), Sc (307), and the remaining REEs, titanium, and zinc (238–71.5; 99; 98). Under highly acidic solutions, however, the TSIL only showed affinity for thorium but not for the remaining species. The metal-...
Release time:
2026
-
03
-
18
viewed:18